Grade Finder

Search the full grade index by designation, standard, equivalent or application.

Every grade we document

8 grades found

Duplex 2205

Duplex 2205

UNS S31803 / S32205EN 1.4462

The most widely used duplex grade. Roughly double the yield strength of 316L, allowing thinner and lighter sections while delivering far better chloride stress corrosion cracking resistance.

6 forms available
Inconel 625

Inconel 625

UNS N06625EN 2.4856

Nickel-chromium-molybdenum alloy strengthened by niobium. Exceptional strength and corrosion resistance from cryogenic temperatures to 980 C without heat treatment.

5 forms available
Inconel 600

Inconel 600

UNS N06600EN 2.4816

Solid solution nickel-chromium-iron alloy with high resistance to oxidation, carburisation and chloride ion stress corrosion cracking at elevated temperature.

5 forms available
Monel 400

Monel 400

UNS N04400EN 2.4360

Nickel-copper alloy with outstanding resistance to flowing seawater, hydrofluoric acid and alkalis, and total immunity to chloride stress corrosion cracking.

5 forms available
Hastelloy C276

Hastelloy C276

UNS N10276EN 2.4819

Nickel-molybdenum-chromium alloy with tungsten, regarded as the most universally corrosion resistant alloy available for both oxidising and reducing media.

5 forms available
316 / 316L

316 / 316L

UNS S31600 / S31603EN 1.4401 / 1.4404

Molybdenum-bearing austenitic stainless steel. The 2-3% Mo addition transforms pitting resistance in chloride-bearing media, making 316L the baseline grade for marine and chemical service in the Gulf.

6 forms available
904L

904L

UNS N08904EN 1.4539

High alloy austenitic grade with 4-5% molybdenum and copper, bridging the gap between 316L and nickel alloys for sulphuric and phosphoric acid service.

5 forms available
Titanium Grade 2

Titanium Grade 2

UNS R50400EN 3.7035

Commercially pure titanium, the industry workhorse. Fully resistant to seawater and oxidising chlorides with excellent formability and weldability.

6 forms available